Ab Initio investigation of chloroaqualead (II) complexes as possible corrosion products in Super Critical Water Cooled Reactor (SCWR)

Main Article Content

D. Anzelj
Cory C. Pye

Abstract

One of the undesirable processes hindering development of Generation IV SCWR is the possibility of corrosion of construction material. Formation of corrosion products such as metal-ligand complexes is poorly understood both experimentally and computationally. It is essential to predict and control its water chemistry to ensure sustainability of SCWR. Pressurized and heated solutions are challenging for experimental research; computational method becomes an important research tool. A series of ab initio calculations of chloroaqualead (II) complexes have been performed at HF, MP2 and B3LYP levels of theory with CEP-121G, LANL2DZ, SDD basis sets for Pb and 6-31G*, 6-31+G*, 6-311+G* for water.

Article Details

Section
Articles